Malmoesoldier
Banned
- Joined
- Nov 13, 2007
- Messages
- 247
The steel was taken somewhere else first, I will let you find it mr researcher, its on this site
All the steel was not recycled, I seen some 2004 when I was in New York
They had no access to the steel and it was recycled quick. but lets say they had access, the steel with the highest temp was still 600C for support columns and 250C for core columns. then its even more proof that the towers shouldnt have collapsed, if they had access to all the steel and couldn't find any with higher temp. But we know the government destroyed the evidence very quick.
From page 8-12 911proof.com/NIST%20DQA%20Petition%20Appeal.pdf
In the original Request, the Requesters challenged NIST’s computer model steel temperatures of 700°C and higher in light of the WTC Report’s statement that NIST’s physical tests on the recovered steel samples “show no evidence of exposure to temperatures above 600°C for any significant time,” and “limited exposure if any above 250°C” (See NCSTAR 1-3, p. xli) (emphasis added). In the Response, NIST suggests that the steel samples saved were intended only for “determining the quality of the steel and, in combination with published literature, for determining mechanical properties as
input to models of building performance.” However, in NIST’s Progress Report of May, 2003 (p. 30), the analysis of recovered steel was explained as a much more involved process, and the goals of the intended analyses were much broader: NIST has catalogued 235 pieces of World Trade Center steel as of March 28, 2003. This includes a database with photographic records and member markings. These pieces represent a small fraction of the enormous amount of steel examined at the various salvage yards where the steel was sent as the WTC site was cleared. In addition, NIST has examined additional steel stored by the Port Authority at JFK airport and has transported 12 specimens to NIST. NIST believes that this collection of steel from the WTC towers is adequate for purposes of the investigation.
The NIST analysis of recovered WTC steel includes:
• collection and cataloging of the structural steel;
• documenting failure mechanisms and damage based on visual observations;
• determining the metallurgical and mechanical properties of steel, weldments, and connections for use in analyzing baseline structural performance, aircraft impact damage, and thermalstructural response to the fires until collapse initiation;
• estimating the maximum temperature reached by available steel;
and
• comparing measured steel properties with applicable material specifications.
The steel in NIST’s possession includes 28 perimeter column panels for
which locations have been identified in the towers, several from the
impact zones; and 11 core columns for which locations have been
identified in the towers, including two from the impact zones.”
NIST also has samples of core columns (wide flange and built-up box
columns) of two grades of steel. Ninety-nine percent of the core columns
were fabricated from these two grades of steel. These statements from the May 2003 progress report were reaffirmed in the December 2003 progress report. (See NIST Special Publication 1000-4, available at wtc.nist.gov/media/PublicUpdateFinal.pdf). Therein, NIST states that it “has in its possession about 236 pieces of WTC Steel”. (See id at p.8) Additionally, “[r]egions of impact and fire damage were emphasized in the selection of steel for the Investigation.” (Id.) “NIST has samples of all 14 grades of steel used in the exterior column-spandrel panels. It also has samples of two grades of steel used for the core columns (wide flange
and built-up box columns) that represent steel used to fabricate 99 percent of the core columns. Most importantly, “NIST believes that this collection of steel from the WTC Towers is adequate for purposes of the Investigation,” which included estimating the maximum temperature reached by the steel. (See id.) (emphasis in original). From these progress reports by NIST, as well as other facts, the Requesters can understand the following:
1. Although the steel samples saved for testing were of limited quantity, an
“enormous amount” of the WTC steel was examined either for or by NIST, and
the samples selected were chosen for their identified importance in the
investigation.
2. Contrary to NIST’s current statement, “estimating the maximum temperature reached by available steel” was stated to be a primary objective of the investigation of the recovered steel samples. This stated objective was repeated in NIST’s December 2003 progress report.
3. Contrary to NIST’s current statement, “documenting failure mechanisms and
damage based on visual observations” was a primary objective of the
investigation. This stated objective was repeated in NIST’s December 2003
progress report.
4. When this sifting and sorting of steel originally occurred, NIST believed “that this collection of steel from the WTC towers [was] adequate for purposes of the
investigation.”
5. In NIST’s December 2003 progress report (p. 8), it was stated that “Regions of impact and fire damage were emphasized in the selection of steel for the Investigation.”
This means that in December 2003 it appears that NIST believed it had adequate samples of steel available to perform physical tests and “estimat[e] the maximum temperature reached by available steel.” Furthermore, the Response also states that “While NIST did not find evidence that any of the recovered core columns experienced temperatures in excess of 250 °C, it is not possible to extrapolate from such a small sample size to state that none of the core columns on the fire affected floors reached temperatures in excess of 250 °C.” NIST’s response here is not satisfactory for the following reasons:
1. It is clear, from NIST’s earlier progress reports, that the steel samples used in the steel temperature analyses were taken from a much larger sample, and represented those areas of the buildings which had experienced significant fire and damage.
2. NIST has not shown any evidence that the steel available to the investigation team was of a “small sample size”. In fact, the 11 core column samples saved could be reasonably seen as representing as much as 23% of the total (47) core columns. Without a detailed explanation from NIST as to how the samples were saved from the larger amount examined, and how the calculation of 1% was performed, the public cannot validate NIST’s new claim that the samples were insufficient to accomplish the original stated objectives, including the maximum steel temperature determination.
3. As with NIST’s new statements about the floor tests, noted above, the Requesters must now ask – Why did NIST perform the steel temperature tests, including the paint deformation test and the tests of steel microstructure, if the results would not be used in the final analyses? Will the American public be refunded the money spent on these tests?
4. The paint deformation test that NIST performed, and that resulted in the 250 °C value discussed, appears to be a measure of the surface temperature of the steel samples tested. NIST provides no explanation for how such a surface temperature result could have been extrapolated to provide meaningful data about the temperature of large masses of core columns, floor assemblies and exterior columns in the WTC towers. In order to validate NIST’s new claim that the test results cannot be extrapolated to provide meaningful information, the details of the intended extrapolation protocol must be provided for public use. Indeed, it is difficult to imagine how a surface temperature of 250°C could be extrapolated in such a way that the inner temperature of the steel could ever have been greater than 250°C.
5. In November of 2004, one of the Requesters sent a letter to Dr. Frank Gayle of NIST, asking for information on the steel temperature tests performed, and the conclusions drawn from the results of those tests. This letter was never answered, but the October 2004 NIST WTC presentation, on which the letter was based, repeatedly stated that large quantities of the steel in the towers had “softened”. After receiving this letter, NIST delayed their report and removed the word “softened” from throughout their descriptions of the collapse initiation sequences. These facts indicate that NIST did not have any plan for extrapolating the results of steel temperature tests, and have never had a scientific basis for the claims made in the NIST WTC report about steel temperatures.